| (IS : 3038-1965, IS : 2856-1964) | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Grades | Tensile strength, Min. kgf/mm2 | Elongation percent Min. | Yield stress or 0.5% proof stress Min. kgf/mm2 | C % | Si % | Mn % | S % | P % | Typical Applications |
| 1 | 55 | 17 | 35 | 0.2-0.25 | 0.15-4.4 | 1.25-1.45 | 0.05 | 0.05 | Cast parts which are to withstand temperatures 300o-525o C |
| 2 | 47 | 17 | 25 | 0.25 Max. | 0.2-0.5 | 0.5-1 | 0.05 | 0.05 | |
| 3 | 52 | 15 | 31 | 0.15 Max. | 0.4 Max. | 0.4-0.8 | 0.05 | 0.05 | |
| 4 | 49 | 17 | 28 | 0.2 Max. | 0.6 Max. | 0.5-0.8 | 0.05 | 0.05 | |
| 5 | 52 | 17 | 31 | 0.08-0.15 | 0.35 Max. | 0.3-0.7 | 0.05 | 0.05 | |
| 6 | 63 | 15 | 43 | 0.2 Max. | 0.75 Max. | 0.4-0.7 | 0.05 | 0.05 | |
| 7 | 63 | 15 | 43 | 0.2 Max. | 1.0 Max. | 0.3-0.7 | 0.05 | 0.05 | |
| CSw-20 | 42 | 20 | 21 | 0.25 Max. | 0.6 Max. | 0.7 Max. | 0.05 | 0.05 | Parts to be fusion welded |
| CSw-25 | 49 | 18 | 25 | 0.3 Max. | 0.6 Max. | 1.0 Max. | 0.05 | 0.05 | |