Injection molding makes most of the plastic parts around you, from bottle caps to car dashboards. Granules of plastic are melted, forced into a closed mold under pressure, cooled until solid, and pushed out as a finished part. The cycle repeats every few seconds. This article walks through each stage, the parameters that matter, and a worked example of shot weight and output.
The machine and the mold
An injection molding machine has two halves. The injection unit melts and injects the plastic: a screw turns inside a heated barrel, conveying granules forward as they soften and then melt. The clamping unit holds the two mold halves together against the injection pressure and opens them for ejection. The mold itself is a precision tool with the cavity that shapes the part, channels (sprue, runners and gates) that feed the melt, cooling lines that remove heat, and ejector pins that push the part out.
The cycle, stage by stage
- Plasticizing: the screw rotates and draws melt forward, building a pool of plastic at the screw tip. Back pressure keeps the melt uniform.
- Clamping: the clamping unit closes the mold and locks it with the clamping force.
- Injection (filling): the screw pushes forward like a piston, forcing melt through the nozzle, runners and gates into the cavity. This stage takes about one to a few seconds.
- Packing (holding): pressure is held on the melt to feed extra material into the cavity as it starts to shrink. Packing continues until the gate freezes.
- Cooling: the part cools in the closed mold until it is stiff enough to eject. Cooling is usually the longest stage, often half the cycle or more.
- Ejection: the mold opens and the ejector pins push the part out. The mold closes and the cycle starts again.
Parameters that control quality
| Parameter | Typical role |
|---|---|
| Melt temperature | Too low gives short shots and poor surface; too high degrades the polymer. |
| Mold temperature | Controls surface finish, warpage and cooling time. |
| Injection pressure and speed | Must fill the cavity before the melt freezes; affects weld lines and stress. |
| Holding pressure and time | Feeds material to offset shrinkage; affects sink marks and weight. |
| Cooling time | Sets most of the cycle time; depends on wall thickness and material. |
| Clamping force | Keeps the mold closed against cavity pressure; too little gives flash. |
Definitions and units
- Shot weight: the total mass injected per cycle, parts plus runner system, in grams.
- Cycle time: the time for one complete cycle, in seconds.
- Cavity: one shaped impression in the mold; a multi-cavity mold makes several parts per cycle.
- Density: mass per unit volume of the molded material, in g/cm³. Polypropylene is about 0.90 to 0.91 g/cm³.
Assumptions
- The part volume and material density are known, and the molded part is fully dense.
- The runner weight is estimated separately and stays constant per cycle.
- The stage times are machine settings or measurements, and the machine runs without stoppages.
Worked example: shot weight and output rate
Given: a two-cavity mold making a small polypropylene container. Each part has a volume of 45 cm³, PP density is 0.905 g/cm³, and the runner system weighs 12 g per shot. The stage times are injection 1.5 s, packing 5 s, cooling 12 s, and mold open, eject and close 4 s.
Step 1, part weight: 45 cm³ × 0.905 g/cm³ = 40.7 g per part.
Step 2, shot weight: 2 × 40.7 + 12 = 93.5 g per cycle.
Step 3, cycle time: 1.5 + 5 + 12 + 4 = 22.5 s.
Step 4, output: 3600 ÷ 22.5 = 160 cycles per hour, so 160 × 2 = 320 parts per hour.
Quick lesson: cooling dominates this cycle at 12 s of 22.5 s. Halving the wall thickness would cut the cooling time roughly by a factor of four, because cooling time grows with the square of the wall thickness.
Limitations
Real molding adds detail this overview skips: drying hygroscopic materials like nylon and polycarbonate, gate freeze studies, mold flow simulation for filling balance, and trial runs to tune the process. The stage times above are illustrative; actual times come from the part design, material data sheet and machine trials. Defects such as warpage, sink marks, weld lines and short shots each have their own causes and remedies.
Try the calculators
- Injection Molding Cycle Time Calculator for the full cycle from its stages.
- Injection Molding Shot Weight Calculator for shot size from part and runner.
- Injection Molding Cooling Time Calculator for cooling time from wall thickness.
- Injection Molding Clamping Force Calculator for the required machine tonnage.
- Injection Molding Cost Calculator for cost per part.
- Plastic Moisture Content Calculator for drying checks.